Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Elastron V201.A40.B - TPV - Elastron Kimya A.S.

Material Data Center offers the following functions for Elastron V201.A40.B:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Elastron V datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ASTM Data
Contracción posterior al moldeo, paralelo 0.0321 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.0126 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Esfuerzo de fractura a tracción 3.2 MPa ASTM D 638
Alargamiento a la rotura 550 % ASTM D 638
Módulo en 100% alargamiento 1.8 MPa ASTM D 412
Módulo en 300% alargamiento 2.5 MPa ASTM D 412
Dureza A Shore 40 - ASTM D 2240
Resistencia al desgarro 16 kN/m ASTM D 624
Compresión residual, 22 hr @ 73 °F 19 % ASTM D 395
Compresión residual, 22 hr @ 158 °F 27 % ASTM D 395
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Combustibilidad UL 94 HB - UL 94
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 920 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Forma de suministro
Negro
Características especiales
Estable contra rayos U.V./interperie, Estable contra el calor
Características
Textura suave
Resistencia quimica
Resistencia al ozono
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.